Skip to main content
. Author manuscript; available in PMC: 2024 Mar 1.
Published in final edited form as: Macromol Biosci. 2022 Dec 21;23(3):e2200425. doi: 10.1002/mabi.202200425

Table 1.

Viscosity of polymers used in hydrogel formation at 37 °C. Viscosities of HA, HANor, and HATet at 2, 4, and 6% w/v.

Polymer 2% w/v [mPa s] 4% w/v [mPa s] 6% w/v [mPa s]
HA 3.3 ± 0.7 17.3 ± 2.7 76.2 ± 10.2
HANor 3.1 ± 0.5 16.4 ± 2.4 37.8 ± 5.6
HATet 2.4 ± 0.4 15.1 ± 1.7 36.3 ± 4.7