Table 1.

Design of experiment.

Sample no Radius(mm) Laydown speed (cm/s) No. of repass
1–15 1000, 800, 600, 400, 200 5.08 0
16–30 400 2.54, 5.08, 7.62, 10.16, 12.7 0
31–39 600, 400, 200 5.08 0, 1, 2

HGT temperature: 875°C, HGT flow rate: 0.06 m3/min, and Compaction Force: 266.89 N.