. 2023 Mar 19;16(6):2451. doi: 10.3390/ma16062451

Figure 6.

Figure 6

Battery performances of the samples in half-cells in 1 M LiPF6 in EC: DEC (1:1) with 10% FEC and 2% VC electrolyte. First cycles at C/20 with the corresponding irreversible capacities for Si-GHG samples (a) and Si@C-GHG samples (b). Cycling performances (discharge capacities) of the different samples at C/5 charging/discharging rate (c).