Table 2.
Samples | ΔL% | ||||
---|---|---|---|---|---|
Elongation | UTS | Breaking Point | Yield Strength | Young’s Modulus | |
Mepilex Lite® | 26.17 ± 8.84 | 305.14 ± 54.10 **** | 272.33 ± 7.49 *** | 0.58 ± 0.07 | 202.9286 ± 50.85 * |
Biatain® Alginate | - | - | - | - | - |
Biofiber | 28.18 ± 1.51 ** | 26.64 ± 14.66 | -3.077 ± 1.58 | 0.41 ± 0.089 | 2661.70 ± 890.37 **** |