Skip to main content
. 2023 Mar 11;16(6):2257. doi: 10.3390/ma16062257

Figure 12.

Figure 12

Crack patterns of straight BCSF-reinforced UHPC specimens with varying content of 1–6 wt.% at 28 days after flexural strength test: (a) 1%; (b) 2%; (c) 3%; (d) 4%; (e) 5%; (f) 6%.