Figure 8

Mechanical properties of WAAM Al-Cu alloys with different Cu contents after T6 heat treatment. 5.0-H and 5.0-V are the horizontal and vertical mechanical properties of the deposit with 5.0% Cu content after T6 heat treatment, respectively; 5.65-H and 5.65-V are the horizontal and vertical mechanical properties of the deposit with 5.65% Cu content after T6 heat treatment, respectively; 6.3-H and 6.3-V are the horizontal and vertical mechanical properties of the deposit with 6.3% Cu content after T6 heat treatment, respectively.