Skip to main content
. 2023 Mar 29;9(4):281. doi: 10.3390/gels9040281

Table 2.

Values of the root mean square roughness for XG-based composite hydrogels.

Scanning Area 1 5 × 5 μm2 10 × 10 μm2 20 × 20 μm2 30 × 30 μm2 40 × 40 μm2
XGVII 17 ± 0.2 18 ± 1 22 ± 8 42 ± 2 63 ± 1
XG90F.III 23 ± 1 25 ± 1 30 ± 4 40 ± 3 46 ± 5
XG50F.III 76 ± 12 85 ± 5 92 ± 2 95 ± 3 98 ± 1

1 All the data were expressed as the mean ± standard deviation (SD).