Skip to main content
. 2023 Mar 29;9(4):281. doi: 10.3390/gels9040281

Table 3.

The experimental results of n′, n″, m, A, and R2 values of XG-based composite hydrogels.

Sample G0′ (Pa) n′ n″ −m R2 (G′) R2 (|η*|)
CG90F.III 766 ± 15 0.026 0.020 −0.974 0.652 0.999
CG90F.V 399 ± 8 0.093 0.066 −0.907 0.944 0.999
CG90F.VII 1003 ± 21 0.033 0.056 −0.965 0.574 0.999
CG75F.III 582 ± 10 0.087 0.115 −0.912 0.912 0.999
CG75F.V 313 ± 5 0.121 0.085 −0.881 0.968 0.999
CG75F.VII 305 ± 4 0.130 0.100 −0.871 0.967 0.999