Figure 6.

Figure 6

Cross-sections of the PLA + bronze specimens after fracture observed by means of a stereoscopic microscope, magnification ×12; (a) specimen 4.0 2Z, with visible black areas indicating lack of filament (1); (b) specimen 4.0 5Y; (c) specimen 1.0 2Z; (d) specimen 1.8 5X.