Skip to main content
. 2023 Apr 20;16(8):3241. doi: 10.3390/ma16083241

Figure 9.

Figure 9

Cross-section of specimen 4.0 2Z composed of PLA + bronze after fracture observed with a scanning electron microscope. Observation direction—perpendicular to the cross-section; (a) magnification ×25; (b) magnification ×100; (c) magnification ×500.