Depolymerization of [PMMA-I]0 (3.2 mM) in tetraglyme. GPC traces obtained from the samples: before reaction (black line); reacted at 120 °C for 24 h with TACP-I as catalyst (red line); reacted at 150 °C for 24 h with TACP-I as catalyst (blue line). Figure adapted with permission from Royal Society of Chemistry from ref (68), copyright 2022; permission conveyed through Copyright Clearance Center, Inc.