. 2023 Apr 22;16(9):3299. doi: 10.3390/ma16093299

Figure 12.

Figure 12

A SEM image and oxidization scheme of the base-X samples with compositions 1–5 after high-temperature oxidation resistance testing at 1150 °C during 30 h. An arrow shows the visible depth of the oxidized layer.