Table 6.
No. | base+X alloy | Fitting Equation | Weight Gain, g/m2 |
---|---|---|---|
1 | +2.5Mo-0.5%Re-0.5%Ta | y = 0.0002x3 − 0.0076x2 + 0.231x + 2.2869 | 7.282 |
2.1 | +2.5Mo-1.5%Re-1.5%Ta | y = 23.084ln(x) + 45.958 | 133.624 |
2.2 | +2.5Mo-1.5%Re-1.5%Ta (TVT *) | y = − 0.0295x2 + 2.3405x + 3.6274 | 48.372 |
3 | +2.5Mo-1.5%Ta-1.5%La-0.5%Ru | y = 0.0002x3 − 0.0094x2 + 0.165x + 1.096 | 2.772 |
4 | +2.5Mo-1.5%Re-1.5%Ta-0.2%Ti | y = −0.044x2 + 3.1537x + 0.3412 | 55.886 |
5 | +2.5Mo-1.5%Re-1.5%Ta-0.2%Zr | y = −0.0295x2 + 2.593x + 5.6503 | 57.546 |
*—TVT—thermo-vacuum treatment.