Skip to main content
. 2023 Apr 25;15(9):2033. doi: 10.3390/polym15092033

Figure 3.

Figure 3

SEM images of the tensile fracture surfaces of the specimens: (a) CF/PA-PU, (b) 1%Gr/CF/PA-PU, and (c) 5%LCP/CF/PA-PU composites. The SEM images of (d,e) are taken at high magnification of (c) and (a).