Skip to main content
. 2023 May 6;15(9):2205. doi: 10.3390/polym15092205

Figure 3.

Figure 3

Modulated DSC curves. The reversible (top left) curves show most of the melting (endothermic). The non-reversible curves (bottom left) show enthalpic relaxation (endothermic), cold crystallization (exothermic), and some of the melting (endothermic), which all occur around the same temperature. The total (right) curves are a combination of the reversible and non-reversible curves and equivalent with unmodulated DSC.