Table 2.
Molecular weight, surface tension, critical aggregation concentration, and thermal stability characterization of CN-OHglcPASs.
| Polymer | [Mo]/[I] | Mn, theory (kDa) | Mn,NMR (kDa) | NNMR | Yield % | Surface tension (mN/m) | CAC (μM) | Tdeccomposition (°C) |
|---|---|---|---|---|---|---|---|---|
| C14-OHglcPAS-12 | 12 | 2.48 | 1.91 | 9 | 76 | 41.3 | 3.3 | 243.3 |
| C14-OHglcPAS-25 | 25 | 4.94 | 3.17 | 15 | 34 | 49.5 | 10.1 | 258.3 |
| C16-OHglcPAS-12 | 12 | 2.50 | 1.56 | 7 | 44 | 45.3 | 8.0 | 250.3 |
| C16-OHglcPAS-25 | 25 | 4.96 | 3.42 | 11 | 17 | 45.4 | 1.8 | 252.9 |
| C18-OHglcPAS-12 | 12 | 2.53 | 1.40 | 6 | 77 | 52.1 | 8.9 | 245.6 |
| C18-OHglcPAS-25 | 25 | 4.99 | 3.48 | 17 | 57 | 51.2 | 1.8 | 252.6 |
| OHglcPAS-25 | 25 | 4.7 | 6.04 | 32 | 70 | 69.6 | >1000 | 230.0 |
Mn= number average molecular weight, N= number of monomer repeat units, Đ = dispersity.