The effects of the post-processing washing cycles on PCL–M polyHIPEs, (A) the decrease in diameter and (B) the percentage decrease in diameter and length of cylindrical scaffolds (n = 16, black dots represent data points). (C) The significant changes in stiffness of PCL–M polyHIPEs following post-processing washing cycles could be visually observed when loads ranging from 0–50 g were applied (scale bar = 1 cm).