Mechanical properties of biodegradable prostheses before and after drug loading in comparison with the sheep carotid artery.

Sample N Tensile Strength, MPa
Me
(25–75%)
Elongation, %
Me
(25–75%)
Young’s Modulus, MPa
Me
(25–75%)
Sheep carotid artery 14 1.2
(1.06–1.9)
158.5
(126.0–169.5)
0.49
(0.39–0.66)
PHBV/PCL 7 3.99
(3.71–4.23)
1438.0
(1403.0–1510.0)
11.52
(10.66–12.21)
PCL 7 5.84
(5.56–6.13)
1391.0
(1350.0–1413.0)
9.33
(9.23–9.55)
PHBV/PCL/PVP 7 3.61
(3.23–4.01)
1202.0
(1120.0–1298.0) *,●
19.8
(18.23–20.9) *,●
PCL/PVP 7 3.75
(3.48–4.01) *,●
1183.0
(1157.0–1215.0) *,●
12.86
(11.86–14.06) *,●
PHBV/PCL/PVP/Ilo/A 7 3.89
(3.88–3.99)
1364.0
(1343.0–1393.0) *,●
14.55
(13.22–15.24) *,●
PCL/PVP/Ilo/A 7 4.02
(3.80–4.18) *,●
1454.0
(1433.0–1458.0) *,●,▲
10.15
(9.82–10.57) *,●,▲

Note: *—p < 0.05 in comparison with PHBV/PCL or PCL; •—p < 0.05 in comparison with sheep carotid artery; ▲—p < 0.05 in comparison with PHBV/PCL/PVP or PCL/PVP. Data are presented as the median (Me) and interquartile range (25–75%).