Skip to main content
. 2023 May 12;15(10):2294. doi: 10.3390/polym15102294

Figure 3.

Figure 3

Reflection spectra and photographs of the gel-immobilized colloidal photonic crystal films with an NIPAM mole fraction of x = 0.4 immersed in elastomer precursor solutions with PEPA concentrations of (A) 0 wt.%, (B) 20 wt.%, (C) 33 wt.%, (D) 36 wt.%, (E) 50 wt.%, and (F) 70 wt.% at each process ((a) before and (b) after the solvent replacement and (c) after UV light irradiation). The length of the scale bar in the photographs is 1 mm.