Table 3. Crystallinity of AKM/PEEK composite specimens.
ω (AKM = 0 wt%) | ω (AKM = 5 wt%) | ω (AKM = 10 wt%) | ω (AKM = 15 wt%) | |
---|---|---|---|---|
∆Hm (J/g) | 45.20 | 37.85 | 34.45 | 32.40 |
Xc (%) | 34.77 | 29.12 | 26.50 | 24.92 |
ω (AKM = 0 wt%) | ω (AKM = 5 wt%) | ω (AKM = 10 wt%) | ω (AKM = 15 wt%) | |
---|---|---|---|---|
∆Hm (J/g) | 45.20 | 37.85 | 34.45 | 32.40 |
Xc (%) | 34.77 | 29.12 | 26.50 | 24.92 |