Table II.
Two-Point Bend Test Experiment Matrix
| Alloy | Heat Treated | NaCl-Na2SO4 Salted | Surface treatment | Heat Treatment Time (h) at 550 °C | ||
|---|---|---|---|---|---|---|
| Grit Blasted | Vapour Aluminised | Pack Aluminised | ||||
| CMSX-4 | √ | N/A | ||||
| √ | √ | 100 | ||||
| √ | √ | 124* | ||||
| √ | √ | √ | 124* | |||
| √ | √ | 124* | ||||
| √ | √ | √ | 100 | |||
| √ | √ | √ | √ | 100 | ||
| √ | √ | √ | 100 | |||
| RR3010 | √ | √ | √ | 100 | ||
| √ | √ | 100 | ||||
| √ | √ | 100 | ||||
| √ | √ | √ | 100 | |||
| √ | √ | 100 | ||||
| √ | √ | 100 | ||||
| √ | √ | √ | 100 | |||
| √ | √ | √ | 100 | |||
*Some samples were heat treated for longer due to covid-19 pandemic-related lab access restrictions.