Skip to main content
. 2023 May 30;2023:9624637. doi: 10.1155/2023/9624637

Table 2.

Temperature program employed in the determination of Cd and Pb in the digestates of polyurethane foam by GF AAS.

Step T (°C) Ramp (s) Hold (s) Ar flow rate (L·min−1)
Drying I 95 10.0 0.3

Drying II 140 12.0 20.0 0.3

Pyrolysisa 700 (Cd) 5.0 5.0 0.3
1000 (Pb)

Atomizationa 1800 (Cd) 2.0 1.0 (Cd) 0.0
2000 (Pb) 2.0 (Pb)

Cleaning 2000 (Cd) 5.0 0.3
2100 (Pb)

aOptimum temperatures of pyrolysis and atomization were set by analyzing the profile of the respective curves (see text for details).