Table 3. Saturation Magnetization (Ms), (Mr), and Hci (Oe) of the FeCoNiAlMn1–xCrx HEAP Milled for 45 h and Vacuum-Heated at 500 °C for 4 h.
| sample (x mole) | Ms (emu/g) | Mr (emu/g) | Hci (Oe) |
|---|---|---|---|
| 0.0 | 62.92 | 4.06 | 178.21 |
| 0.2 | 64.60 | 3.31 | 130.52 |
| 0.4 | 68.15 | 3.16 | 132.02 |
| 0.6 | 68.91 | 3.08 | 151.48 |
| 0.8 | 64.63 | 4.84 | 187.51 |
| 1.0 | 51.91 | 5.18 | 192.01 |