. 2023 May 22;39(22):7731–7740. doi: 10.1021/acs.langmuir.3c00554

Table 3. Images, Water Contact Angle Measurements, and Sliding Angle Measurements for the 0.5PDMS/SiO2/0.5(SA+PA)/40 and 0.5PDMS/SiO2/0.5FAS/40 Films after Heating at 300 °C for 5 h and 400 °C for an Additional 5 h.

graphic file with name la3c00554_0011.jpg