Table 1.
The performance of LABs with different SSEs.
Composites | Initial Capacity (mAh g−1) (Current Density) |
End of Capacity (mAhg−1) (Cycle Number) |
Ionic Conductivity (S cm−1) /Temperature |
Type | Reference |
---|---|---|---|---|---|
LLZTO/PPC/LiTFSI | 20,300/20 μA cm−2 | -/(50) | 1.6 × 10−3/RT | ISE | [27] |
ZSM-5 | -/400 mA g−1 | 70/480 | - | ISE | [53] |
UFSLAGP | 152.2/(0.1 C) | -/31 | 1.6 × 10−3/RT | ISE | [60] |
LAGP@glass | 414/0.1 A g−1 | 142.5/120 | 9.85 × 10−4/60 °C | ISE | [56] |
S-CPE | 123/- | 404.89/100 | - | CPE | [68] |
PMMA-LiTFSI | 159.6/(0.1 C) | -/5 | 2.80 × 10−4/RT | GPE | [69] |
PVAN50−20%LATP−10%SN | 140/34 mA g−1 | 156.9/30 | 1.13 × 10−4/RT | CPE | [63] |
PVDF/HEC/PVDF | 6019/100 mA g−1 | 125/140 | 0.88 × 10−4/RT | GPE | [74] |
PFPE@PVDF-HFP | -/0.1 mA cm−2 | -/1200 h | - | SPE | [75] |
PI@GPE | 2485/0.05 mA cm−2 | -/366 | 0.44 × 10−4/RT | CPE | [79] |
3D-CPE | 7540/312.5 mA g−1 | 1786/3 | 9.2 × 10−5/RT | CPE | [80] |
PSSE/GPE | 173/24 mA g−1 | -/194 | 1.06 × 10−3/RT | CPE | [81] |
LiBH4-MgO | 35,111/50 mA g−1 | 162/5 | 2.86 × 10−4/RT | ISE | [86] |
PMMA/m-MgO | 153.0/0.5 C | -/52 | 7.76 × 10−4/RT | CPE | [87] |
PVDF-HFP/PMMA ZrO2-6% (PPZ-6%) | 120/0.1 A g−1 | 151.0/200 | 1.46 × 10−3/RT | CPE | [88] |
PEO-TiO2 SnO2@LATP |
157.6/0.1 C - |
119/50 142.1/200 |
3 × 10−4/70 °C - |
CPE ISE |
[89] [99] |