Table 3.
Strain Rate [s−1] | Young’s Modulus [kPa] | (ΔR/R)max | Elasticity | Plateau | Densification | |||
---|---|---|---|---|---|---|---|---|
Sε | Sσ | Sε | Sσ | Sε | Sσ | |||
0.01 | 19.63 | 17.17% | 0.487 | 0.025 kPa−1 | 0.223 | 0.077 kPa−1 | −0.411 | −0.026 kPa−1 |
0.1 | 22.881 | 13.89% | 0.446 | 0.019 kPa−1 | 0.211 | 0.074 kPa−1 | −0.454 | −0.026 kPa−1 |
1 | 31.058 | 10.76% | 0.334 | 0.008 kPa−1 | 0.141 | 0.037 kPa−1 | −0.436 | −0.02 kPa−1 |
10 | 32.35 | 9.97% | 0.287 | 0.002 kPa−1 | 0.112 | 0.044 kPa−1 | −0.413 | −0.005 kPa−1 |