Skip to main content
. 2023 May 30;15(11):2525. doi: 10.3390/polym15112525

Figure 12.

Figure 12

SEM images of the fracture surface after tensile testing of the 3D-printed PLA–PDA–KF: (a) PLA–PDA–KF5 (500 µm); (b) PLA–PDA–KF5 (250 µm); (c) PLA–PDA–KF5 (50 µm); (d) PLA–PDA–KF10 (500 µm); (e) PLA–PDA–KF10 (250 µm); (f) PLA–PDA–KF10 (50 µm); (g) PLA–PDA–KF15 (500 µm); (h) PLA–PDA–KF15 (250 µm); (i) PLA–PDA–KF15 (50 µm); (j) PLA–PDA–KF20 (500 µm); (k) PLA–PDA–KF20 (250 µm); and (l) PLA–PDA–KF20 (50 µm).