Table 1. Particle Size of Silybin Suspensions after High-Pressure Homogenization and Ball Milling.

pretreatment method particle size (nm) PDI
homogen 0 cycles 1397.7 ± 214.0 0.994
homogen 4 cycles 705.5 ± 66.8 0.385
homogen 8 cycles 600.9 ± 53.6 0.143
homogen 12 cycles 552.5 ± 40.9 0.209
ball-milling 0 h 1147.3 ± 175.1 0.932
ball-milling 1 h 362.4 ± 10.1 0.403
ball-milling 2 h 355.6 ± 4.1 0.343
ball-milling 3 h 318.9 ± 4.0 0.293