Skip to main content
. 2023 May 11;24(6):2706–2720. doi: 10.1021/acs.biomac.3c00156

Figure 8.

Figure 8

(A) Hydrogen-bond density versus strain and temperature (pure, dry cellulose). (B–D) Hydrogen-bond density versus degree of ring opening at 0% strain at different temperatures and water contents. (C, D) Same as (B) at 50 and 100% strain, respectively.