Min Max Mean Median SD
Bracket group A: stainless steel
ΔF −21.10 −6.90 −10.37 −9.44 3.61
ΔQ −17.70 −0.10 −3.16 −1.34 4.22
Bracket group B: titanium
ΔF −18.60 −6.85 −10.61 −9.70 3.10
ΔQ −8.66 −0.03 −1.46 −0.61 1.91
Bracket group C: ceramic
Pixels −17.70 −6.97 −9.49 −8.74 2.50
Pixels × area −12.20 −0.010 −2.17 −1.05 3.02

ΔF fluorescence loss (%), ΔQ fluorescence loss × area (% × mm2), SD standard deviation, Min minimum, Max maximum