Heat Treatment protocols applied to the parallelepiped IN718 and IN718-NbC samples fabricated via LBP-DED.

Heat Treatment As-DED A B
Sample(s) All A Samples B Samples
Temperature /°C - 720 / 620 1100
Time / min - 480 / 480 120
Cooling - Air Air
Notes Machined Condition Two stage ppt treatment ReX