Table 4.
Activation energies of subbands detected in Cu2O single-crystal samples (obtained with an error of ≈15%).
Sample |
Ea, eV 660 nm |
Ea, eV 680 nm |
Ea, eV 720 nm |
Ea, eV 810 nm |
Ea, eV 920 nm |
|
---|---|---|---|---|---|---|
Cu2O single crystal @ laser irradiation power |
SC (111) @ 0.2 mW |
80 | 150 | |||
SC (111) @ 15 mW |
93 | 190 | ||||
SC (100) @ 0.2 mW |
89 | 22 | 135 | |||
SC (100) @ 15 mW |
97 | 20 | 197 | |||
Cu2O thin films | 111 | 32 | 77 | 42 | 15 + 37 | |
13 | 36 | 43 | 62 | 65 | ||
30 | 41 | 59 | 33 | 22 | ||
39 | 59 | 86 | 37 | 12 + 126 | ||
40 | 32 | 40 | 55 | 37 | 18 + 247 |