. 2023 Jun 9;23(12):5469. doi: 10.3390/s23125469

Table 3.

Measurement results of different standard samples.

Sample Name Thickness (mm) Density (g/cm3) Resonant Frequency Point (GHz) HPPFD (GHz) Permittivity Loss Tangent
Quartz 1.50 2.20 10.0437 0.0059 4.1 4.7 × 10−4
PTFE 1 2.00 2.28 10.0581 0.0037 2.1 6.9 × 10−4
PTFE 2 3.00 2.24 9.9391 0.0056 2.0 4.5 × 10−4
Silicon oxide ceramics 1.96 1.57 10.0126 0.0276 3.0 3.7 × 10−3