. 2021 Jun 30;104(2):00368504211029469. doi: 10.1177/00368504211029469

Figure 10.

Figure 10.

Microstructure of the Al–Mg–Si alloy with different wt.% of Al–5Ti–1B grain refiner (GR) specimens after corrosion test in 3.5 wt% NaCl solution: (a) 0 wt% GR, (b) 1% GR, (c) 1.5% GR, and (d) 2% GR.