Table 2. Pure Epoxy Resin and Different Proportions of Silicone Modification.
| n(silicone):n(EA) | T50% (°C) | Tmax (°C) | residue (%) |
|---|---|---|---|
| 0 | 421.89 | 424.33 | 8.3447 |
| 0.1:1 | 424.33 | 428.33 | 7.5148 |
| 0.2:1 | 424.78 | 427.67 | 5.5766 |
| 0.3:1 | 423.79 | 430.33 | 8.2051 |
| 0.4:1 | 419.23 | 424.33 | 8.0885 |
| 0.5:1 | 424.80 | 430.33 | 8.5411 |