Scoring Standard of Lane-Sandhu Histological Scoring Method for Bone Defect Repair

Evaluation Criteria Score
No connections 0
Fiber connection 1
Bone connectivity Connection of bone and osteoid 2
Bone junction 3
Complete regeneration of diaphysis 4
No osteocyte activity 0
Early aggregation of new bone 1
Cancellous bone Active new bone aggregation 2
Cancellous bone is being transformed 3
Complete formation of cancellous bone 4
No cortical bone growth 0
Early manifestations of cortical bone growth 1
Cortical bone Cortical bone is forming 2
Most of the cortical bone is modified 3
Complete bone regeneration 4