Figure 3.
(a) Relationship between Young’s modulus E at 300 K and the reciprocal of mean grain size d−1 of polycrystalline U-10Mo alloys. (b) Variations in yield strength and UTS with the reciprocal of the square root of the mean grain size d−1/2. (c) Evolution of fractions of atoms in grain cores and grain boundaries with the reciprocal of mean grain size d−1. (d) Relationship between Young’s modulus and fraction of atoms in grain cores.