Table 3.
Comparison of peak-to-peak values of principal strain between single sheet and column region of laminated core under different magnetization conditions (μm/m).
IDC = 0 A | 1.4 T | 1.5 T | 1.6 T | 1.7 T |
---|---|---|---|---|
single sheet | 1.11 | 1.27 | 1.47 | 1.54 |
laminated core | 1.22 | 1.43 | 1.72 | 2.19 |
amplification | 9.9% | 12.5% | 17.0% | 42.2% |
I DC = 0.1 A | 1.4 T | 1.5 T | 1.6 T | 1.7 T |
single sheet | 1.40 | 1.57 | 1.72 | 1.77 |
laminated core | 1.54 | 1.76 | 1.98 | 2.44 |
amplification | 10.1% | 12.1% | 15.1% | 38% |
I DC = 0.2 A | 1.4 T | 1.5 T | 1.6 T | 1.7 T |
single sheet | 1.58 | 1.72 | 1.80 | 1.84 |
laminated core | 1.76 | 1.94 | 2.32 | 2.576 |
amplification | 11.3% | 12.8% | 28.8% | 40% |