Skip to main content
. 2023 Jul 3;8(28):25020–25033. doi: 10.1021/acsomega.3c01644

Table 2. Comparison of Prepared Bi2O3-WO3/rGO NCs with Some Reported Samples in the Degradation of Rhodamine B (RhB) Dye.

sample used conc. and amount of sample UV light source irradiation time (min) D (%) references
Bi2O3/WO3 NCs/rGO NC 10 ppm, 35 mg 400 W (Xenon lamp) 180 91 present work
WO3/Ag/CN NCs 10 ppm, 10 mg 400 W (Xenon lamp) 140 96.2 (58)
TiO2@SiO2/WO3/GO NCs 10 ppm, 25 mg 500 W (Xenon lamp) 50 98 (59)
TiO2-Ag2O/rGO NCs 10 ppm, 35 mg 350 W (Xenon lamp) 60 92 (60)
MoS2/Bi2O2CO3 NCs 10 ppm, 50 mg 500 W (Mercury lamp) 150 92 (61)
WO3/TNTs NCs 10 ppm, 40 mg 400 W (Xenon lamp) 60 91.8 (62)
Ag/β-Ag2WO4/WO3 NCs 10 ppm, 30 mg 350 W (Xenon lamp) 25 99.6 (63)
MoO3-Bi2O3/rGO NC 10 ppm, 40 mg 300 W (Xenon lamp) 120 80 (64)