FIGURE 2.
(A) Temperature-dependent Rheological curves for the prepared CH (B) Temperature changes of CuP NPs at various concentrations under a 5 min irradiation from a 1,064 nm laser at 0.5 W/cm2 (C) Heating curve of CH for four cycles having a 0.5 W/cm2 power intensity under irradiation by 1,064 nm laser (D) SEM image of the CH (E) The photographic pictures represent the morphology of the prepared CH and IR image during laser irradiation (F) Relevant 3D temperature diagram in 2 E.