Table 2.
Thermal properties of F2 and F5.
| Sample | T5 (◦C) | T10 (◦C) | T50 (◦C) | Tmax (oC) | Char yield at 600 °C (%) |
|---|---|---|---|---|---|
| F2 | 362 | 374 | 397 | 401 | 1.98 |
| F5 | 364 | 377 | 395 | 400 | 0.67 |
Thermal properties of F2 and F5.
| Sample | T5 (◦C) | T10 (◦C) | T50 (◦C) | Tmax (oC) | Char yield at 600 °C (%) |
|---|---|---|---|---|---|
| F2 | 362 | 374 | 397 | 401 | 1.98 |
| F5 | 364 | 377 | 395 | 400 | 0.67 |