Spherulites diameter and roughness of the sample (Sa) after cooling from melt.
| Copolymer | Spherulite diameter [µm] | Sample roughness (Sa) |
|---|---|---|
| PHF-DLF | 4.5 | 24 |
| POF-DLF | 4.0 | 37 |
| PDF-DLF | 6.0 | 63 |
| PDDF-DLF | 8.0 | 42 |
| Copolymer | Spherulite diameter [µm] | Sample roughness (Sa) |
|---|---|---|
| PHF-DLF | 4.5 | 24 |
| POF-DLF | 4.0 | 37 |
| PDF-DLF | 6.0 | 63 |
| PDDF-DLF | 8.0 | 42 |