. 2023 Jul 24;13:11915. doi: 10.1038/s41598-023-39203-5

Table 6.

TGA and DTG information of nanocomposites.

Samples Temperature at 5% weight loss (T5) First degradation temperature (T1max) Final degradation temperature (T2max) Ash content at 700 °C (wt%)
R 448 408 665 35.7
R-BN1% 449 382 670 36.17
R-BN3% 450 395 660 37.48
R-BN5% 454 440 660 41.5
R-sBN1% 415 372 600 36.52
R-sBN3% 412 362 590 36.86
R-sBN5% 403 360 570 37.42