Table 2. Average elastic recovery and strain in compression of commercial and experimental VPS immediately after setting.
| Impression materials | Elastic recovery (%) | Strain-in- compression |
|---|---|---|
| Aq M | 99.32 ± 0.30 | 4.261 ± 0.154 |
| Elt M | 99.31 ± 0.35 | 3.153 ± 0.177 |
| Extr M | 99.27 ± 0.32 | 4.405 ± 0.118 |
| Exp-I | 99.32 ± 0.52 | 4.677 ± 0.207 |
| Exp-II | 99.65 ± 0.09 | 5.360 ± 0.163 |
| Exp-III | 99.50 ± 0.23 | 6.137 ± 0.256 |
| Exp-IV | 99.37 ± 0.26 | 6.541 ± 0.239 |
| Exp-V | 99.12 ± 0.16 | 7.076 ± 0.220 |