Weight loss measurements of thermoplastic polyurethane polycaprolactone (PLC-TPU) and TPU based on fatty acid dimers after 2 months of incubation at 30 °C with different molds. Control: material incubated in the absence of molds. Adapted from Ref. [46] which is an open access article under the terms of the Creative Commons Attribution License (http://creativecommons.org/licenses/by/4.0/).