Skip to main content
. 2023 Jul 24;16(14):5192. doi: 10.3390/ma16145192

Figure 2.

Figure 2

PDP curves for X60-Steel in pickling solution (HCl) with different FSG6-6 concentrations (A) and the occurrence of 0.2 mM of different surfactants (B) at 50 °C.