. 2023 Jul 9;13(14):2035. doi: 10.3390/nano13142035

Figure 5.

Figure 5

Comparison of bacterial adhesion between bare PU foam and FSCSN-coated PU foam through quantitative results after exposure to bacteria for (a) 1 h and (b) 8 h.