Normalized ethane loading in 20 defective MOFs at room temperature. Each loading is normalized to the loading in the associated defect-free structure at the same pressure and is displayed using a log scale. (a) Normalized isotherms averaged over 20 MOFs; color bar represents the log10 (uptake ratio); (b) uptake ratio distribution of 20 MOFs at 2.5 defect concentration. (c) Uptake ratio distribution of 20 MOFs at a defect concentration of 10 defect concentration.