Skip to main content
. 2023 Jul 31;13:12381. doi: 10.1038/s41598-023-39347-4

Figure 2.

Figure 2

(a) Cross-sectional topogram 30 μm below from the surface (left) and sagittal topogram at the orange line (right). (b) Intensity line profiles at stacking faults indicated by green line in sagittal topogram (top) and at screw dislocation indicated by green circle in cross-sectional topogram (bottom).