Table 10. Average plastic strain components (in microstrain) for the Cu phase of the two-phase model for ΔT = 70°C; there was no plastic flow in the W grains.

Parameter Inline graphic Inline graphic Inline graphic Inline graphic Inline graphic Inline graphic
Average −5 2 4 −14 3 1
Standard deviation 13 54 55 167 3 1
Maximum 84 187 365 798 15 4